Mechanical Properties Metric English Comments
Tensile Stress 25.6 MPa

@Strain 0.250 %,
Temperature 0.000 °C
3710 psi

@Strain 0.250 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..
Tensile Stress 25.6 MPa

@Strain 4.60 %,
Temperature 90.0 °C
3710 psi

@Strain 4.60 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr..
Tensile Stress 25.6 MPa

@Strain 0.240 %,
Temperature -40.0 °C
3710 psi

@Strain 0.240 %,
Temperature -40.0 °F
ISO 527
DuPont Performance Polymers Rynite® 408 NC010 PET
Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf..