Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 36.61 MPa @Strain 3.06 %, Temperature 180 °C |
5310 psi @Strain 3.06 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) 40% Glass/Mineral Reinforced Polyamide 66 Zytel FE270038 is a 40% glass fiber/mineral reinforced heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.I.. |