Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 36.17 MPa @Strain 0.340 %, Temperature 23.0 °C |
5246 psi @Strain 0.340 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |