Polymer Property : Tensile Stress = 3526 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 24.31 MPa

@Strain 0.210 %,
Temperature 0.000 °C
3526 psi

@Strain 0.210 %,
Temperature 32.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)
Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance ..