Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 35.26 MPa @Strain 7.41 %, Temperature 40.0 °C |
5114 psi @Strain 7.41 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |