Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 23.95 MPa @Strain 0.490 %, Temperature 90.0 °C |
3474 psi @Strain 0.490 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough.. |
|||
Tensile Stress | 23.95 MPa @Strain 0.290 %, Temperature 40.0 °C |
3474 psi @Strain 0.290 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66
(Unverified Data**) 43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |