Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 22.4 MPa @Strain 0.470 %, Temperature 150 °C |
3250 psi @Strain 0.470 %, Temperature 302 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Tensile Stress | 22.4 MPa @Strain 0.800 %, Temperature 40.0 °C |
3250 psi @Strain 0.800 %, Temperature 104 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66
(Unverified Data**) Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 22.4 MPa @Strain 3.00 %, Temperature 160 °C |
3250 psi @Strain 3.00 %, Temperature 320 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |