Mechanical Properties Metric English Comments
Tensile Stress 22.11 MPa

@Strain 0.220 %,
Temperature 90.0 °C
3207 psi

@Strain 0.220 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)  (Unverified Data**)
Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed ..