Mechanical Properties Metric English Comments
Tensile Stress 3.84 MPa

@Strain 300 %
557 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® A9860M TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Stress 3.84 MPa

@Strain 300 %
557 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® F7860 TPE, Fire Retardant
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome..
Tensile Stress 3.84 MPa

@Strain 0.0300 %,
Temperature 40.0 °C
557 psi

@Strain 0.0300 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de..
Tensile Stress 3.84 MPa

@Strain 60.07 %,
Temperature 100 °C
557 psi

@Strain 60.07 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 3.84 MPa

@Strain 147.11 %,
Temperature 120 °C
557 psi

@Strain 147.11 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 3.84 MPa

@Strain 39.75 %,
Temperature 100 °C
557 psi

@Strain 39.75 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..