Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.62 MPa

@Strain 300 %
525 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® A9845 TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Stress 3.62 MPa

@Strain 300 %,
Temperature 23.0 °C
525 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7670-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7670-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..