Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.48 MPa @Strain 133.39 %, Temperature 120 °C |
505 psi @Strain 133.39 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |