Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 20.3 MPa @Strain 300 % |
2950 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Uniprene® UN-7010-40D-NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Tensile Stress | 20.34 MPa @Strain 0.100 %, Temperature 23.0 °C |
2950 psi @Strain 0.100 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |