Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 28.73 MPa @Strain 1.18 %, Temperature 180 °C |
4167 psi @Strain 1.18 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)
(Unverified Data**) Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed .. |