Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 28.5 MPa @Strain 50.0 %, Temperature 120 °C |
4130 psi @Strain 50.0 %, Temperature 248 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66
(Unverified Data**) Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 28.5 MPa @Strain 3.00 %, Temperature 23.0 °C |
4130 psi @Strain 3.00 %, Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66
(Unverified Data**) Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 28.5 MPa @Strain 0.330 %, Temperature 40.0 °C |
4130 psi @Strain 0.330 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |