Tensile Stress 1.88 MPa

@Strain 300 %,
Temperature 23.0 °C
273 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2706-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA and medical compliance. - High Puncture Reseal - Overmold Adhesion to Po..
Tensile Stress 1.88 MPa

@Strain 0.000 %,
Temperature -20.0 °C
273 psi

@Strain 0.000 %,
Temperature -4.00 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..