Mechanical Properties Metric English Comments
Tensile Stress 27.4 MPa

@Strain 0.240 %,
Temperature 0.000 °C
3970 psi

@Strain 0.240 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough..