Mechanical Properties Metric English Comments
Tensile Stress 27.22 MPa

@Strain 0.430 %,
Temperature 120 °C
3948 psi

@Strain 0.430 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Rynite® FR543 NC010 PET
Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm..
Tensile Stress 27.22 MPa

@Strain 1.66 %,
Temperature 40.0 °C
3948 psi

@Strain 1.66 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6  (Unverified Data**)
15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per..
Tensile Stress 27.22 MPa

@Strain 0.270 %,
Temperature 40.0 °C
3948 psi

@Strain 0.270 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica..