Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 17.9 MPa

@Strain 5.00 %,
Temperature 23.0 °C
2600 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® BM6574 BK316 TPC-ET  (Unverified Data**)
Hytrel® BM6574 is a 65 nom. Shore D, plasticiser free high performance resin for blow molding and extrusion; it shows ageing resistance up to 150°C, and excellent mechanical properties at elevated..
Tensile Stress 17.9 MPa

@Strain 300 %,
Temperature 23.0 °C
2600 psi

@Strain 300 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET  (Unverified Data**)
Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio..