Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 26.27 MPa @Strain 17.4 %, Temperature 40.0 °C |
3810 psi @Strain 17.4 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |