Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 26.12 MPa @Strain 0.215 %, Temperature -20.0 °C |
3788 psi @Strain 0.215 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |