Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 17.88 MPa @Strain 90.5 %, Temperature 60.0 °C |
2593 psi @Strain 90.5 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |