Polymer Property : Tensile Stress = 25166 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 173.51 MPa

@Strain 1.39 %,
Temperature 23.0 °C
25166 psi

@Strain 1.39 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA)
35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e..