Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 25.71 MPa @Strain 18.63 %, Temperature 40.0 °C |
3729 psi @Strain 18.63 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide.. |