Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 17.13 MPa @Strain 0.200 %, Temperature -20.0 °C |
2485 psi @Strain 0.200 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica.. |