Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 16.7 MPa @Strain 0.460 %, Temperature 150 °C |
2420 psi @Strain 0.460 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough.. |
|||
Tensile Stress | 16.7 MPa @Strain 0.530 %, Temperature 23.0 °C |
2420 psi @Strain 0.530 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |