Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 24.579 MPa @Strain 0.8588 %, Temperature 0.000 °C |
3564.9 psi @Strain 0.8588 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |