Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.60 MPa @Strain 100 % |
232 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G50A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 1.60 MPa @Strain 100 % |
232 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G50A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 1.60 MPa @Strain 100 % |
232 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G50D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 1.60 MPa @Strain 100 % |
232 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |