Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 23.17 MPa @Strain 0.240 %, Temperature 90.0 °C |
3361 psi @Strain 0.240 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica.. |