Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 15.63 MPa @Strain 270.58 %, Temperature 120 °C |
2267 psi @Strain 270.58 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |