Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 22.2 MPa @Strain 0.630 %, Temperature 120 °C |
3220 psi @Strain 0.630 %, Temperature 248 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |