Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 148.08 MPa @Strain 1.00 %, Temperature -40.0 °C |
21477 psi @Strain 1.00 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66
(Unverified Data**) 43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |