Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 203.2 MPa @Strain 2.28 %, Temperature -20.0 °C |
29470 psi @Strain 2.28 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35EF NC010 Nylon 66 + Nylon 6
(Unverified Data**) 35% Glass Reinforced Polyamide 66 Developed for Electrical and Electronics ApplicationsZytel 70G35EF NC010 is a 35% glass reinforced polyamide 66 developed for electrical and electronics application.. |