Mechanical Properties Metric English Comments
Tensile Stress 203 MPa

@Strain 3.00 %
29400 psi

@Strain 3.00 %
Solvay TECHNYL® A 218 V30 Black 21 NHFE PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218 V30 BLACK 21NHFE is a polyamide 6.6, high flow, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Be..