Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 13.84 MPa @Strain 0.410 %, Temperature 150 °C |
2007 psi @Strain 0.410 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica.. |