Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 138 MPa @Strain 1.50 %, Temperature -40.0 °C |
20000 psi @Strain 1.50 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Tensile Stress | 138 MPa @Strain 1.50 %, Temperature 0.000 °C |
20000 psi @Strain 1.50 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 138 MPa @Strain 1.76 %, Temperature 23.0 °C |
20000 psi @Strain 1.76 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Tensile Stress | 138 MPa @Strain 0.100 % |
20000 psi @Strain 0.100 % |
Process Temperature T4 |
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - .. |