Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.52 MPa @Strain 300 % |
365 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C4850 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 2.52 MPa @Strain 100 %, Temperature 21.0 °C |
365 psi @Strain 100 %, Temperature 69.8 °F |
Across Flow 2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Tensile Stress | 2.52 MPa @Strain 0.0600 %, Temperature -20.0 °C |
365 psi @Strain 0.0600 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica.. |