Tensile Stress 2.45 MPa

@Strain 100 %,
Temperature 21.0 °C
355 psi

@Strain 100 %,
Temperature 69.8 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ HC 9210-70N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-70N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items and soft-touch overmolding for surgical grips. Product ex..
Tensile Stress 2.45 MPa

@Strain 300 %
355 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP-2815A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Stress 2.45 MPa

@Strain 0.100 %,
Temperature 150 °C
355 psi

@Strain 0.100 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G15HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR NC010 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..