Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.31 MPa @Strain 300 % |
335 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® D6840 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Stress | 2.31 MPa @Strain 300 %, Temperature 23.0 °C |
335 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE) Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Tensile Stress | 2.31 MPa @Strain 300 %, Temperature 23.0 °C |
335 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ 9555-9 Thermoplastic Elastomer (TPE) Versaflex™ 9555-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Tensile Stress | 2.31 MPa @Strain 300 %, Temperature 23.0 °C |
335 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Prod.. |
|||
Tensile Stress | 2.31 MPa @Strain 300 %, Temperature 23.0 °C |
335 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versalloy™ XL 9055-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Tensile Stress | 2.31 MPa @Strain 300 %, Temperature 23.0 °C |
335 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versalloy™ XL 9055X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Overmold Adhesion to Polypro.. |
|||
Tensile Stress | 2.31 MPa @Strain 300 % |
335 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3857CT TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |