Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 13.26 MPa @Strain 36.85 %, Temperature 100 °C |
1923 psi @Strain 36.85 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |