Polymer Property : Tensile Stress = 19039 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 131.27 MPa

@Strain 1.25 %,
Temperature -20.0 °C
19039 psi

@Strain 1.25 %,
Temperature -4.00 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor..
Tensile Stress 131.27 MPa

@Strain 1.30 %,
Temperature 40.0 °C
19039 psi

@Strain 1.30 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35EF BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN51G35EF BK083 is a 35% glass reinforced heat stabilized lubricated high performance..
Tensile Stress 131.27 MPa

@Strain 1.30 %,
Temperature 40.0 °C
19039 psi

@Strain 1.30 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..