Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 19.84 MPa @Strain 2.50 %, Temperature 80.0 °C |
2878 psi @Strain 2.50 %, Temperature 176 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |