Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 12.9 MPa @Strain 100 % |
1870 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3897 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 12.89 MPa @Strain 0.400 %, Temperature 23.0 °C |
1870 psi @Strain 0.400 %, Temperature 73.4 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 12.9 MPa @Strain 0.700 %, Temperature 23.0 °C |
1870 psi @Strain 0.700 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |