Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 12.8 MPa @Strain 100 % |
1860 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3895 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 12.8 MPa @Strain 0.940 %, Temperature 150 °C |
1860 psi @Strain 0.940 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Tensile Stress | 12.8 MPa @Strain 240.5 %, Temperature 150 °C |
1860 psi @Strain 240.5 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |