Tensile Stress 127 MPa

@Strain 1.30 %,
Temperature 0.000 °C
18400 psi

@Strain 1.30 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi..
Tensile Stress 127 MPa

@Strain 1.52 %,
Temperature 0.000 °C
18400 psi

@Strain 1.52 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers