Mechanical Properties Metric English Comments
Tensile Stress 12.6 MPa

@Strain 300 %
1830 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-88-N809C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Stress 12.62 MPa

@Strain 0.220 %,
Temperature 0.000 °C
1830 psi

@Strain 0.220 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66  (Unverified Data**)
20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf..
Tensile Stress 12.6 MPa

@Strain 0.270 %,
Temperature 40.0 °C
1830 psi

@Strain 0.270 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66  (Unverified Data**)
30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa..
Tensile Stress 12.6 MPa

@Strain 300 %
1830 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ P55D-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P55D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 12.6 MPa

@Strain 300 %
1830 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ P55D-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P55D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..