Polymer Property : Tensile Stress = 1819 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 12.54 MPa

@Strain 0.130 %,
Temperature -20.0 °C
1819 psi

@Strain 0.130 %,
Temperature -4.00 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica..
Tensile Stress 12.54 MPa

@Strain 0.100 %,
Temperature 23.0 °C
1819 psi

@Strain 0.100 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m..