Mechanical Properties Metric English Comments
Tensile Stress 12.16 MPa

@Strain 147.28 %,
Temperature 120 °C
1764 psi

@Strain 147.28 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET  (Unverified Data**)
82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers