Polymer Property : Tensile Stress = 176.66 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 176.66 MPa

@Strain 1.55 %,
Temperature -20.0 °C
25622 psi

@Strain 1.55 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo..
Tensile Stress 176.66 MPa

@Strain 2.29 %,
Temperature 23.0 °C
25622 psi

@Strain 2.29 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G35HSLR BK031 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR BK031 is a 35% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..