Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 17.14 MPa @Strain 2.03 %, Temperature 150 °C |
2486 psi @Strain 2.03 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |