Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.20 MPa @Strain 100 % |
1625 psi @Strain 100 % |
Average; ASTM D412 Method A |
Seals Eastern 7265 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Vito.. |